MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD 6733.17 Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable production of products free of taste and odor for food and beverage packaging.

Availability: Latin America, North America and South America

Additive:

  • Antioxidant: Yes
Applications:
  • Food Packaging Containers
  • Food Service Trays
  • Houseware Articles
  • Housewares
  • Toys
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D4883
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 190 °C
33 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.44 MPa3400 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Flexural Modulus 0.965 GPa
@Strain 2 %
140 ksi
@Strain 2 %
Secant; ASTM D790
Izod Impact, Notched 0.224 J/cm
@Temperature -40.0 °C
0.420 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C153 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C100 °FASTM D648
 
Descriptive Properties
FeaturesStandard Processing Antioxidants Stabilizer
FormPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 6719.17 Injection Molding Resin
ExxonMobil HD 6719.62 Injection Molding Resin
ExxonMobil HD 6605.70 Injection Molding Resin
ExxonMobil HD 6706.62 Injection Molding Resin
Dow DOWLEX™ IP-41 High Density Polyethylene

PEXB071 / 37376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.