MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® XE 4181 nat PA1010
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grilamid XE 4181 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 natural is highly resistant to automotive fluids and chemicals in general. Unique features of Grilamid XE 4181 natural are:
  • Polymer fully based on renewable raw materials
  • Flexibility, high elongation
  • Very low water absorption
  • Good cold impact resistance
  • Good heat and UV resistance
  • Excellent chemical and zinc-chloride resistance
  • Easy processing
Application examples: Grilamid XE 4181 natural has been designed for use in various types of demanding automotive and industrial tubings. It is technically a very close and bio based alternative to comparable PA12 based Grilamid products.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccDry; ISO 1183
Water Absorption 1.3 %Sim. to ISO 62
Moisture Absorption 0.700 %Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 35.0 MPaConditioned; ISO 527-1/-2
 40.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 30 %Dry; ISO 527-1/-2
 30 %Conditioned; ISO 527-1/-2
Tensile Modulus 600 MPaConditioned; ISO 527-1/-2
 800 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 55.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 70.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+8 ohm-cmConditioned; IEC 60093
 1.00e+9 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 37.0 kV/mmConditioned; IEC 60243-1
 39.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 170 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-1/-2
Melting Point 197 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Fuel systems
 Hydraulic systems
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingOther Extrusion
Product AttributesBio based Polyamide
 Flexible
 High viscosity
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® 1SVX-65H nat PA1010-GF65
EMS-Grivory Grilamid® 1SVX-50H nat PA1010-GF50
EMS-Grivory Grilamid® XE 4116 nat PA1010-GF55
EMS-Grivory Grilamid® XE 4180 nat PA1010
Techmer ES Luriblend® PE 5903

PGRH145 / 156854

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.