MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® XE 4180 nat PA1010
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grilamid XE 4180 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 NATURAL is highly resistant to automotive fluids and chemicals in general. Unique features of Grilamid XE 4180 NATURAL are:
  • Polymer fully based on renewable raw materials
  • High flexibility, high elongation
  • Very low water absorption
  • Good cold impact resistance
  • Good heat and UV resistance
  • Excellent chemical and zinc-chloride resistance
  • Easy processing
Application examples: Grilamid XE 4180 natural has been designed for use in various demanding automotive and industrial tubings. It is technically a very close and bio based alternative to comparable PA12 based Grilamid products.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³Dry; ISO 1183
Water Absorption 1.5 %1.5 %Sim. to ISO 62
Moisture Absorption 0.600 %0.600 %Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Conditioned; ISO 527-1/-2
Tensile Modulus 0.480 GPa69.6 ksiConditioned; ISO 527-1/-2
 0.600 GPa87.0 ksiDry; ISO 527-1/-2
50% Modulus  30.0 MPa
@Strain 50 %
30.0 MPa
@Strain 50 %
Dry; ISO 527-1/-2
 30.0 MPa
@Strain 50 %
30.0 MPa
@Strain 50 %
Conditioned; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cmDry; IEC 60093
 1.00e+9 ohm-cm1.00e+9 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Strength 35.0 kV/mm889 kV/inDry; IEC 60243-1
 35.0 kV/mm889 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 170 µm/m-°C94.4 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
Melting Point 194 °C381 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Compressed air systems
 Exterior
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Lighting
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesBio based Polyamide
 Improved flowability and demolding
Special CharacteristicsHigh impact or impact modified
 Improved UV resistance (outdoor use)
 Light stabilized or stable to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® 1SVX-65H nat PA1010-GF65
EMS-Grivory Grilamid® 1SVX-50H nat PA1010-GF50
EMS-Grivory Grilamid® XE 4116 nat PA1010-GF55
EMS-Grivory Grilamid® XE 4181 nat PA1010
Overview of materials for Nylon 6, 50% Glass Fiber Filled

PGRH143 / 156852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.