MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Surlyn® 9720 Ionomer Resin, Zinc
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutralization levels for this grade are optimized to deliver low temperature toughness, plus abrasion resistance and stiffness. For wire and cable applications, this grade contains an antioxidant and meets Mil Spec P46124 MR, Type V, Class I requirements. The resin can be injection or blow molded, and is processable by extrusion into sheets or shapes.

Data provided by the manufacturer.

This former DuPont product line is now a Dow product line.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D2240
Tensile Strength, Ultimate 30.3 MPa4390 psiASTM D638
Tensile Strength, Yield 11.7 MPa1700 psi50 mm/min cross speed; ASTM D638
Elongation at Break 440 %440 %ASTM D638
Flexural Modulus 0.250 GPa36.3 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Tensile Impact Strength 1260 kJ/m²600 ft-lb/in²ASTM D1822S
Tear Strength 102 kN/m582 pliDie C; ASTM D624
Abrasion 410410NBS Index; ASTM D1630
 
Thermal PropertiesMetricEnglishComments
CTE, linear 160 µm/m-°C
@Temperature -20.0 - 32.0 °C
88.9 µin/in-°F
@Temperature -4.00 - 89.6 °F
ASTM D696
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Melting Point 92.0 °C198 °FDTA
Deflection Temperature at 0.46 MPa (66 psi) 43.0 °C109 °FASTM D648
Vicat Softening Point 71.0 °C160 °FRate B, ASTM D1525-70
Brittleness Temperature -110 °C-166 °FASTM D746
Flame Spread 25.4 mm/min1.00 in/minASTM D635
 
Optical PropertiesMetricEnglishComments
Haze 12 %
@Thickness 6.35 mm
12 %
@Thickness 0.250 in
ASTM D1003A
Gloss 25 %25 %20° per ASTM D523-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 9520 Ionomer Resin, Zinc
Dow Surlyn® 9650 Ionomer Resin, Zinc
Dow Surlyn® 9721 Ionomer Resin, Zinc
Dow Surlyn® 9910 Ionomer Resin, Zinc
Dow Surlyn® 8140 Ionomer Resin, Sodium

PDU418 / 33069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.