MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Garlock GYLON® 3545 Layered Microcellular PTFE Gasketing
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Microcellular PTFE gasket with rigid PTFE core
  • Highly compressible PTFE outer layers seal under low bolt load- suitable for many non-metallic flanges
  • Compressible layers conform to surface irregularities, especially on warped, pitted or scratched flanges
  • Rigid PTFE core reduces cold flow and creep normally associated with conventional PTFE gaskets
Media: Strong caustics, strong acids, hydrocarbons, chlorine and cryogenics.
Conforms to FDA regulations.

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.05 g/ccestimated by MatWeb
Permeability 0.015Gas Permeability, cc/min; DIN 3535 Part 4
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 244 V/mil
@Temperature 121 °C,
Time 10800 sec
0.125 in. thickness; ASTM D149
 248 V/mil
@Temperature 121 °C,
Time 10800 sec
0.0625 in. thickness; ASTM D149
 222 V/mil
@Thickness 1.59 mm
100% RH for 96 hours; ASTM D149
 264 V/mil
@Thickness 3.17 mm
100% RH for 96 hours; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
@Pressure 8.27 MPa
Continuous
Minimum Service Temperature, Air -450 °F
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorWhite
Compressibility, %70-85ASTM F36
Creep Relaxation, %10ASTM F38
Sealability ASTM F37B, ml/hr0.15ASTM Fuel A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1070 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
Struktol STRUKSILON 8018 Silicone Stabilizer for PU-Microcellular Foam
Northstar Polymers MSB-M25B Microcellular Foam based on High Performance Polyester Polyurethane
Mitsubishi Chemical Advanced Materials Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
DIAB ProBalsa® LD7 Light Weight Balsa Wood

PGARL821 / 157498

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.