MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Astralloy 8000® Abrasion-Resistant Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Astralloy 8000® is an advanced abrasion-resistant steel with a good compromise between abrasion resistance and toughness (crack resistance) in extreme applications. It has a wear life which is over 50% higher than 500 HB conventional water quenched steels. Astralloy 8000 capitalizes on an innovative metallurgical concept, based on a specific chemical analysis. This chemical analysis is combined with a dedicated heat treatment conducted by oil quenching. The successful use of Astralloy 8000 for wear parts in various industries is a result of:
  • a superficial hardening following a very efficient work hardening capability in service, governed by a metallurgic phenomenon called TRIP effect (Transformation Induced by Plasticity).
  • a very fine and homogeneous dispersion of hard particles in steel (mainly chromium, molybdenum and titanium microcarbides) giving the material its extremely high abrasion resistance
Astralloy 8000 processes (forming, machining) much better than the existing 500 HB resistant steels. Astralloy 8000 is known as the best compromise for severe applications where exceptional abrasion, impact, heat and moderate corrosion are requested in service. Astralloy 8000 is currently used in industries such as mining, quarries, cement and concrete, iron making, steel processing, recycling, earthmoving, and dredging.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 430 - 470430 - 470
Tensile Strength 1630 MPa236000 psi
Tensile Strength, Yield 1080 MPa156000 psi
Elongation at Break 12 %
@Thickness 50.8 mm
12 %
@Thickness 2.00 in
in 2 in. (50 mm)
Charpy Impact 29.8 J22.0 ft-lb
Bend Radius, Minimum 4.0 t4.0 tParallel to Grain Rolling Direction
 5.0 t5.0 tPerpendicular to Rolling Direction
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.2 µm/m-°C
@Temperature 20.0 - 100 °C
6.22 µin/in-°F
@Temperature 68.0 - 212 °F
 12.0 µm/m-°C
@Temperature 20.0 - 200 °C
6.67 µin/in-°F
@Temperature 68.0 - 392 °F
 12.5 µm/m-°C
@Temperature 20.0 - 300 °C
6.94 µin/in-°F
@Temperature 68.0 - 572 °F
 13.2 µm/m-°C
@Temperature 20.0 - 400 °C
7.33 µin/in-°F
@Temperature 68.0 - 752 °F
 13.8 µm/m-°C
@Temperature 20.0 - 500 °C
7.67 µin/in-°F
@Temperature 68.0 - 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.28 %<= 0.28 %
Chromium, Cr <= 1.6 %<= 1.6 %
Iron, Fe >= 95.9 %>= 95.9 %As Balance
Manganese, Mn <= 1.6 %<= 1.6 %
Molybdenum, Mo <= 0.20 %<= 0.20 %
Nickel, Ni <= 0.40 %<= 0.40 %
Phosphorus, P <= 0.015 %<= 0.015 %
Sulfur, S <= 0.0020 %<= 0.0020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Astralloy 4800® Wear Resistant Steel
Astralloy EB-450® Steel
Astralloy Astralloy-V® Air Hardened Wear Steel Plate
AISI 1117 Steel, annealed at 855°C (1575°F)
AISI 1015 Steel, annealed at 870°C (1600°F), furnace cooled 17°C (31°F) per hour to 725°C (1340°F), air cooled, 25 mm (1 in.) round

NNUCOR901 / 233175

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.