MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4560 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 - 0.900 g/cc0.0217 - 0.0325 lb/in³
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Water Absorption 0.50 %0.50 %ISO 62
Moisture Absorption at Equilibrium 0.25 %0.25 %ISO 62
Viscosity Measurement  70
@Temperature 290 °C
70
@Temperature 554 °F
20 mins plasticating
 75
@Temperature 300 °C
75
@Temperature 572 °F
10 mins plasticating
 75
@Temperature 280 °C
75
@Temperature 536 °F
30 mins plasticating
 90
@Temperature 270 °C
90
@Temperature 518 °F
30 mins plasticating
 95
@Temperature 290 °C
95
@Temperature 554 °F
10 mins plasticating
 100
@Temperature 260 °C
100
@Temperature 500 °F
30 mins plasticating
 100
@Temperature 300 °C
100
@Temperature 572 °F
5 mins plasticating
 105
@Temperature 280 °C
105
@Temperature 536 °F
10 mins plasticating
 106
@Temperature 250 °C
106
@Temperature 482 °F
30 mins plasticating
 110
@Temperature 270 °C
110
@Temperature 518 °F
10 mins plasticating
 115
@Temperature 260 °C
115
@Temperature 500 °F
10 mins plasticating
 115
@Temperature 240 °C
115
@Temperature 464 °F
30 mins plasticating
 117
@Temperature 250 °C
117
@Temperature 482 °F
10 mins plasticating
 120
@Temperature 240 °C
120
@Temperature 464 °F
10 mins plasticating
Viscosity Test 112 cm³/g1.12 dl/gISO 307
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 2577
 0.015 cm/cm0.015 in/inplate with film gate 150x150x3mm3
Linear Mold Shrinkage, Transverse 0.0164 cm/cm0.0164 in/inISO 2577
 0.017 cm/cm0.017 in/inplate with film gate 150x150x3mm3
Melt Flow 42.9 g/10 min
@Load 2.16 kg,
Temperature 250 °C
42.9 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 8.0 %8.0 %50 mm/min; ISO 527-1/-2
 35 %35 %Nominal Strain, 50 mm/min; ISO 527-1/-2
Tensile Modulus 2.60 GPa377 ksiISO 527-1/-2
Flexural Strength 90.0 MPa13100 psiISO 178
Charpy Impact Unnotched  0.850 J/cm²
@Temperature -30.0 °C
4.04 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 14.0 J/cm²
@Temperature 23.0 °C
66.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.380 J/cm²
@Temperature 23.0 °C
1.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Dielectric Constant  3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 130 - 160 µm/m-°C
@Temperature 23.0 - 80.0 °C
72.2 - 88.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Thermal Conductivity 0.270 W/m-K1.87 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 223 °C433 °FISO 11357-1/-2
Maximum Service Temperature, Air 160 °C320 °F
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-1/-2
Decomposition Temperature >= 290 °C>= 554 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Ignition Temperature 350 °C662 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 250 °C482 °FFeeding zone
Zone 2 255 °C491 °FCompression
Zone 3 260 °C500 °FMetering-zone
Zone 4 260 °C500 °FNozzle
Melt Temperature 230 - 275 °C446 - 527 °FInjection molding/Extrusion
 260 °C500 °FOptimal
Mold Temperature 40.0 - 70.0 °C104 - 158 °FInjection molding
 60.0 °C140 °FOptimal
Drying Temperature 80.0 - 120 °C176 - 248 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed< 0.25 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4520 High Speed PBT
BASF Ultradur® B 4406 PBT
BASF Ultradur® B 2550 PBT
BASF Ultradur® B 4500 BK 00110 PBT
BASF Ultradur® B 4500 PBT

PBASG0130 / 131763

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.