MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4500 BK 00110 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes:

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 - 0.900 g/cc0.0217 - 0.0325 lb/in³
Density 1.20 - 1.35 g/cc0.0434 - 0.0488 lb/in³ISO 1183
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°FIEC 1006
Melting Point 220 - 230 °C428 - 446 °FDIN 53736
Decomposition Temperature >= 290 °C>= 554 °F
Ignition Temperature 350 °C662 °FASTM D1929
 
Descriptive Properties
ColorBK 00110
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4500 PBT
BASF Ultradur® B 4520 High Speed PBT
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT
BASF Ultradur® B 4560 PBT
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT

PBASG0121 / 131755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.