MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Excelfrax® 1800 Board Microporous Insulation
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Unifrax Corporation's Excelfrax® microporous insulation technology is a family of products which all exhibit superior insulating characteristics. Excelfrax microporous insulation is composed of inorganic oxides, primarily fumed silica. Silicates and opacifiers are added to improve the material performance. Microporous materials are very efficient insulation products. These products actually have thermal conductivity values lower than still air.

Excelfrax 1800 Board is a high-temperature, rigid, microporous material specifically designed for applications where a strong, highly efficient insulating material is required. Excelfrax 1800 Board is available in thicknesses up to 2" and can be field fabricated to meet specific appliation requirements. Some typical applications for Excelfrax 1800 Board include back-up insulation in high-temperature furnaces (steel, glass, ceramic, aluminum), aluminum launders, and aluminum transfer ladles.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.4 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 1.10 MPaCold Crushing Strength; DIN 51067 / DIN 53421
Compression Set 2.9 %
@Pressure 0.100 MPa
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.800 J/g-°C
@Temperature 32.0 - 800 °C
Thermal Conductivity 0.0190 W/m-K
@Temperature 20.0 °C
DIN 51046
 0.0210 W/m-K
@Temperature 200 °C
DIN 51046
 0.0250 W/m-K
@Temperature 400 °C
DIN 51046
 0.0300 W/m-K
@Temperature 600 °C
DIN 51046
 0.0380 W/m-K
@Temperature 800 °C
DIN 51046
Maximum Service Temperature, Air 1000 °CRecommended Operating Temperature
Minimum Service Temperature, Air 20.0 °CRecommended Operating Temperature
Shrinkage 1.0 %
@Temperature 800 °C
All sides, long term
 4.8 %
@Temperature 1000 °C
All sides, long term
 0.50 %
@Temperature 1000 °C,
Time 43200 sec
Single sided
 
Component Elements PropertiesOriginal ValueComments
SiC 15 %
SiO2 80 %
 
Descriptive Properties
ColorGrey
Other Inorganics (%)5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Anderman Ceramics EREY99 Yttrium Oxide
MarkeTech Silica Aerogel
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation
Pyrotek Pyroboard™ S1300 Roller
Sharadaa Ceramics Resin Bonded Slabs

CUNIF035 / 97807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.