MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SMAC SMACMOUNT® 2528S 04 Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Shock & vibration insulation for:
  • Aircraft avionics components & subassemblies
  • Missile electronics
  • Vehicular electronics requiring vibration isolation
Advantages :
  • Bushing style mount
  • Countersunk for lowest installed height
  • Can be pre-loaded to vary natural frequency
  • Axial to radial stiffness ratio of approx. 1:1

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Load100 N2 mm, Static (Radial) deflection
 150 N5 mm, Static (Compression) deflection
 2 kg60 Hz
 200 N8 mm, Static (Compression) deflection
 200 N5 mm, Static (Radial) deflection
 275 N8 mm, Static (Radial) deflection
 7 kg23 Hz
 90 N2 mm, Static (Compression) deflection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® R 401/10 Silicone Rubber
SMAC SMACMOUNT® 2528S 02 Damping Material
SMAC SMACFOAM® 1250S-01 Damping Material
SMAC BARRIER® Damping Material
Saint-Gobain Korel® K20 Very Soft Micro-cellular Polyurethane Foam

PZSMAC034 / 146150

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.