ELASTOSIL® R 401/10 is a low duro, easily pigmentable silicone rubber base for extrusion and molding applications as well as for manufacturing of silicone sponge articles in combination with peroxide crosslinkers. Special features: ELASTOSIL® R 401/10 is a low duro base but with acceptable to good mechanical as well as good processing properties. It is also suitable as blending component to soften ELASTOSIL® silicone rubber compounds. Application: ELASTOSIL® R 401/10 is suitable for all applications where low hardness, high elongation, good damping etc. are required in combination with typical silicone properties such as very good heat resistance, good release, soft grip etc. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances. Information provided by Wacker Chemie AG. |