MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C15760
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent cold workability. Fabricated by extrusion and drawing.

Applications: resistance welding electrodes, circuit breakers, electrical connectors, wire feed contact tips, plasma spray nozzles, high-strength high temperature parts.

Available as flat products and rod.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/ccC15735
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 486 - 648 MPa
Tensile Strength, Yield 386 - 552 MPaDepending on temper
Elongation at Break 20 %in 203.2 mm.
Tensile Modulus 17000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000220 ohm-cm78% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.20 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 186 BTU-in/hr-ft²-°F
Melting Point 1981 °F
Solidus 1981 °F
Liquidus 1981 °F
Annealing Point 1200 - 1800 °F
 
Component Elements PropertiesOriginal ValueComments
Al2O3 1.1 %
Copper, Cu 98.9 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Bicor™ 19MB440 OPP Film
Copper, UNS C15710
Copper, UNS C15720
Copper, UNS C15735
Copper, UNS C16500

MC15760b1 / 10703

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.