MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C15710
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent cold workability. Fabricated by extrusion, drawing, rolling, impacting, heading, swaging, bending, machining, blanking, roll threading.

Applications: electrical connectors, light-duty current-carrying springs, inorganic insulated wire, thermocouple wire, lead wire, resistance welding electrodes for aluminum, heat sinks.

Available as rod and wire.

Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.82 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 324 - 724 MPa47000 - 105000 psi
Tensile Strength, Yield 268 - 689 MPa38900 - 99900 psiDepending on temper
Elongation at Break 20 %20 %in 254 mm.
Modulus of Elasticity 105 GPa15200 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.5 µm/m-°C
@Temperature 20.0 - 300 °C
10.8 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 360 W/m-K2500 BTU-in/hr-ft²-°F
Melting Point <= 1080 °C<= 1980 °F
Liquidus 1080 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.15 - 0.25 %0.15 - 0.25 %
Copper, Cu 99.69 - 99.85 %99.69 - 99.85 %Specified
Iron, Fe <= 0.010 %<= 0.010 %
Lead, Pb <= 0.010 %<= 0.010 %
Oxygen, O <= 0.040 %<= 0.040 %Excluding Al2O3

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Copper, UNS C12000
Copper, UNS C12100
Copper, UNS C15720
Copper, UNS C15735

MC15710b1 / 10666

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.