MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A. Schulman BMC T15(F) High Strength Grade Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding of intricate parts. Typical applications are circuit breakers, insulators, bobbins and electrical connectors.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 - 2.05 g/cc0.0668 - 0.0741 lb/in³Molded
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 30 - 4030 - 40
Tensile Strength 52.4 - 66.2 MPa7600 - 9600 psi
Flexural Strength 103 - 131 MPa15000 - 19000 psi
Flexural Modulus 7.58 - 8.96 GPa1100 - 1300 ksi
Compressive Strength 124 - 152 MPa18000 - 22000 psi
Izod Impact, Notched 3.04 - 4.11 J/cm5.70 - 7.70 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.3 - 17.3 kV/mm389 - 439 kV/inshort time
Arc Resistance >= 187 sec>= 187 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC T15(GPS) General Purpose Molding Compound
A. Schulman BMC T15(GPT) General Purpose Molding Compound
A. Schulman BMC 5436 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC T15(GP) General Purpose Molding Compound
A. Schulman BMC Super-Tough Mineral Filled, Glass Reinforced Polyester

PBMC932 / 123396

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.