MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain Furon® K271 One-sided Thermal Kapton® Tape
Categories: Polymer; Adhesive; Tape

Material Notes: Description: A 1 mil thermally conductive Kapton® film, coated on one side with 1.5 mils of thermally-conductive acrylic pressure-sensitive adhesive, while the other side is coated with 2 mils of thermally-conductive silicone rubber. Recommended uses: For use in systems where electrical isolation is required and replacement or upgrade of components is common. Application advantages: Kapton provides excellent dielectric strength while minimizing thermal resistance; Excellent for use in small, compact environments where electrical conductivity of interface material can pose a threat; High peel strength adhesion to minimize air entrapment; One-sided adhesive system allows for easy rework. All data based on a 0.0045 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tear Strength 16.0 pliInitial Tear Strength
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.63e+15 ohm-cmASTM D257
Dielectric Strength 1600 V/milASTM D1000
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.500 W/m-KASTM E1530
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -20.0 °F
 
Descriptive Properties
ColorGreen
Thermal Impedance @ 10 psi0.4°C in^2/WASTM E1530

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Furon®, Kapton® K275 Tape
DuPont™ Kapton® HA Polyimide Film
AISI Type 304L Stainless Steel
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness

PSTGQZ481 / 68995

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.