MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Saint-Gobain Furon®, Kapton® K275 Tape
Categories: Polymer; Adhesive; Tape; Thermoplastic

Material Notes: Description: A 1 mil thermally conductive Kapton® film, coated on both sides with 2 mils of thermally-conductive pressure-sensitive adhesive. Recommended uses: Excellent for use in small, compact environments where electrical conductivity of interface material can pose a threat. Application Advantages:
  • Kapton (MT) provides excellent dielectric strength while minimizing thermal resistance
  • High peel strength adhesion to minimize air entrapment
  • Material can be pre-attached to a heat sink or CPU
  • Adverse effects of surface roughness are minimized through a highly conformable pressure-sensitive adhesive
  • Flame Retardant version available
  • Available in slit-rolls or die-cut shapes
All data based on a 0.0045 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tear Strength 2.80 kN/m16.0 pliTensile Strength; ASTM D1000
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.80e+14 ohm-cm3.80e+14 ohm-cmASTM D257
Dielectric Strength 51.2 kV/mm1300 kV/inASTM D1000
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FASTM E1530
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F
 
Descriptive Properties
ColorGreen
Thermal Impedance @ 10 psi0.4°C in^2/WASTM E1530

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kapton® HA Polyimide Film
Saint-Gobain Furon® K271 One-sided Thermal Kapton® Tape
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness
DuPont™ Kapton® 500ZT Polyimide Film, 125 Micron Thickness
DuPont™ Kapton® JP Polyimide Film

PSTGQZ515 / 69029

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.