MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Kapton® 500ZT Polyimide Film, 125 Micron Thickness
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Film thickness 125 micron (5.0 mil)

All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).

General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianhydride with an aromatic diamine. It has excellent chemical resistance; there are no known organic solvents for the film. It does not melt. It can be used at both high and low temperature extremes. Kapton® polyimide films can be used in a variety of electrical and electronic uses: wire and cable tapes, formed coil insulation, substrates for printed circuit boards, motor slot liners, magnet wire insulation, transformer and capacitor insulation, magnetic and pressure-sensitive tapes, and tubing.

Data provided by DuPont High Performance Films.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³
Water Absorption 2.8 %2.8 %24 hr/23°C. ASTM D570
Thickness 3180 microns125 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 75 %75 %Orientation not specified; ASTM D882
Poissons Ratio 0.340.34Value for Kapton® HN
Secant Modulus 2.80 GPa406 ksiASTM D882
Coefficient of Friction, Dynamic 0.480.48Value for Kapton® HN. Film to film. ASTM D1894-90
Coefficient of Friction, Static 0.630.63Kapton® HN. Film to film. ASTM D1894-90
Film Tensile Strength at Break, MD 221 MPa32100 psiOrientation not specified; ASTM D882
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmKapton® HN in damp heat; IPC-TM-650; Method 2.5.17
 1.00e+17 ohm-cm1.00e+17 ohm-cmper ASTM D257-91 for Kapton® HN
Dielectric Constant 3.6
@Frequency 1000 Hz
3.6
@Frequency 1000 Hz
Use evaporated metal electrodes, two terminal system of measurement at standard conditions.; ASTM D150
Dielectric Strength 154 kV/mm3910 kV/inFlat sheets in air; 1/4 in diameter brass electrodes with 0.8 mm edge radius; 60 cps AC at 600V/s; ASTM D149-81
Dissipation Factor 0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
Value for Kapton® HN
 32.0 µm/m-°C
@Temperature 100 °C
17.8 µin/in-°F
@Temperature 212 °F
Value for Kapton® HN
 40.0 µm/m-°C
@Temperature 250 °C
22.2 µin/in-°F
@Temperature 482 °F
Value for Kapton® HN
Specific Heat Capacity 1.09 J/g-°C0.261 BTU/lb-°FValue for Kapton® HN
Thermal Conductivity 0.120 W/m-K0.833 BTU-in/hr-ft²-°FValue for Kapton® HN
Maximum Service Temperature, Air 400 °C752 °FKapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
Minimum Service Temperature, Air -269 °C-452 °FMaintains properties and flexibility
Glass Transition Temp, Tg 385 °C725 °FValue for Kapton® HN
Flammability, UL94 V-0V-0
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.70
@Wavelength 589.3 nm
1.70
@Wavelength 589.3 nm
Value for Kapton® HN.  Na D line; ASTM D542-90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kapton® 500FPC Polyimide Film, 125 Micron Thickness
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness
DuPont™ Kapton® 500VN Polyimide Film, 125 Micron Thickness

PDUK19 / 33389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.