System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Nexeo® HIVAL® 5303 High Impact Polystyrene
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Polystyrene, Impact Modified
Material Notes:
Features:
BPA Free Food Contact
Acceptable
Agency Ratings: FDA 21 CFR 177.1640
RoHS Compliance: RoHS Compliant
Forms: Pellets
Processing:
Method Extrusion
Injection Molding
Information provided by Nexeo® Solutions.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.04
g/cc
ASTM D1505
Melt Flow
3.0
g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
94
ASTM D785
Tensile Strength, Yield
4000
psi
ASTM D638
Tensile Modulus
280000
psi
ASTM D638
Flexural Modulus
280000
psi
ASTM D790
Izod Impact, Notched
3.00
ft-lb/in
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
195
°F
ASTM D648
Vicat Softening Point
200
°F
ASTM D1525
Processing Properties
Original Value
Comments
Rear Barrel Temperature
390
-
450
°F
Injection Molding
Middle Barrel Temperature
400
-
450
°F
Injection Molding
Front Barrel Temperature
425
-
500
°F
Injection Molding
Nozzle Temperature
425
-
500
°F
Injection Molding
Zone 1
380
-
440
°F
Extrusion
Zone 3
390
-
450
°F
Extrusion
Zone 5
400
-
470
°F
Extrusion
Die Temperature
410
-
450
°F
Extrusion
Melt Temperature
425
-
525
°F
Injection Molding
Compliance Properties
Original Value
Comments
FDA
Yes
See notes for details.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Global GP-110 High Impact Polystyrene
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
NIZHNEKAMSKNEFTEKHIM 825 High Impact Polystyrene
Versalis Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR
Overview of materials for Polystyrene, Impact Modified
PNEXEO920 / 197604
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.