MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polystyrene, Impact Modified
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.650 - 2.12 g/cc0.0235 - 0.0766 lb/in³Average value: 1.05 g/cc Grade Count:469
Water Absorption 0.000 - 0.600 %0.000 - 0.600 %Average value: 0.0923 % Grade Count:92
Moisture Absorption at Equilibrium 0.0300 - 0.100 %0.0300 - 0.100 %Average value: 0.0957 % Grade Count:42
Water Absorption at Saturation 0.100 %0.100 %Average value: 0.100 % Grade Count:31
Particle Size 0.800 - 4000 µm0.800 - 4000 µmAverage value: 1240 µm Grade Count:23
Maximum Moisture Content 0.01000.0100Average value: 0.0100 Grade Count:8
Linear Mold Shrinkage 0.00200 - 0.0450 cm/cm0.00200 - 0.0450 in/inAverage value: 0.00597 cm/cm Grade Count:278
Linear Mold Shrinkage, Transverse 0.00200 - 0.00600 cm/cm0.00200 - 0.00600 in/inAverage value: 0.00467 cm/cm Grade Count:3
Melt Flow 0.900 - 99.0 g/10 min0.900 - 99.0 g/10 minAverage value: 7.83 g/10 min Grade Count:524
Spiral Flow 44.0 - 45.0 cm
@Temperature 220 - 220 °C
17.3 - 17.7 in
@Temperature 428 - 428 °F
Average value: 44.5 cm Grade Count:2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 40.0 - 84.040.0 - 84.0Average value: 58.9 Grade Count:69
Hardness, Rockwell M 32.0 - 10332.0 - 103Average value: 66.6 Grade Count:41
Hardness, Rockwell R 53.0 - 12053.0 - 120Average value: 94.2 Grade Count:86
Ball Indentation Hardness 60.0 - 110 MPa8700 - 16000 psiAverage value: 79.5 MPa Grade Count:28
Tensile Strength, Ultimate 12.4 - 240 MPa1800 - 34800 psiAverage value: 26.9 MPa Grade Count:278
Tensile Strength, Yield 2.35 - 200 MPa341 - 29000 psiAverage value: 25.8 MPa Grade Count:388
Elongation at Break 1.30 - 350 %1.30 - 350 %Average value: 45.2 % Grade Count:451
Elongation at Yield 1.00 - 75.0 %1.00 - 75.0 %Average value: 15.3 % Grade Count:87
Modulus of Elasticity 0.155 - 3.47 GPa22.5 - 503 ksiAverage value: 1.97 GPa Grade Count:300
Flexural Yield Strength 3.92 - 450 MPa569 - 65300 psiAverage value: 45.8 MPa Grade Count:343
Flexural Modulus 0.686 - 22.5 GPa99.6 - 3260 ksiAverage value: 2.12 GPa Grade Count:387
Izod Impact, Notched 0.0890 - 9.61 J/cm0.167 - 18.0 ft-lb/inAverage value: 1.14 J/cm Grade Count:405
 0.42712 - 1.81526 J/cm
@Temperature -50.0 - -17.8 °C
0.80017 - 3.40073 ft-lb/in
@Temperature -58.0 - 0.000 °F
Average value: 0.537 J/cm Grade Count:16
 0.0640 - 0.85424 J/cm
@Temperature -30.0 - -18.0 °C
0.120 - 1.6003 ft-lb/in
@Temperature -22.0 - -0.400 °F
Average value: 0.537 J/cm Grade Count:10
 0.0640 - 0.85424 J/cm
@Thickness 3.17 - 6.50 mm
0.120 - 1.6003 ft-lb/in
@Thickness 0.125 - 0.256 in
Average value: 0.537 J/cm Grade Count:10
Izod Impact, Unnotched 0.801 - 5340 J/cm1.50 - 10000 ft-lb/inAverage value: 4.13 J/cm Grade Count:25
Izod Impact, Notched (ISO) 2.00 - 14.0 kJ/m²0.952 - 6.66 ft-lb/in²Average value: 8.35 kJ/m² Grade Count:74
 5.00 - 7.00 kJ/m²
@Temperature -30.0 - -30.0 °C
2.38 - 3.33 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 5.50 kJ/m² Grade Count:2
 3.50 - 6.50 kJ/m²
@Temperature -30.0 - -30.0 °C
1.67 - 3.09 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 5.50 kJ/m² Grade Count:8
 3.50 - 6.50 kJ/m²
@Thickness 4.00 - 4.00 mm
1.67 - 3.09 ft-lb/in²
@Thickness 0.157 - 0.157 in
Average value: 5.50 kJ/m² Grade Count:8
Izod Impact, Unnotched (ISO) 3.00 kJ/m² - NB1.43 ft-lb/in² - NBAverage value: 35.8 kJ/m² Grade Count:33
Charpy Impact Unnotched 0.500 J/cm² - NB2.38 ft-lb/in² - NBAverage value: 7.65 J/cm² Grade Count:83
 2.50 J/cm² - NB
@Temperature -40.0 - -30.0 °C
11.9 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 8.55 J/cm² Grade Count:40
Charpy Impact, Notched 0.110 - 5.00 J/cm²0.524 - 23.8 ft-lb/in²Average value: 0.970 J/cm² Grade Count:88
 0.200 - 0.700 J/cm²
@Temperature -40.0 - -30.0 °C
0.952 - 3.33 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 0.422 J/cm² Grade Count:12
Gardner Impact 1.69 - 36.2 J1.25 - 26.7 ft-lbAverage value: 21.3 J Grade Count:20
Dart Drop, Total Energy 11.3 - 18.0 J8.33 - 13.3 ft-lbAverage value: 14.3 J Grade Count:5
Falling Dart Impact 9.04 - 583 J6.67 - 430 ft-lbAverage value: 55.6 J Grade Count:25
 528.77 - 528.77 J
@Temperature -40.0 - -40.0 °C
390.00 - 390.00 ft-lb
@Temperature -40.0 - -40.0 °F
Average value: 529 J Grade Count:1
Instrumented Impact Total Energy 9.15 - 39.6 J6.75 - 29.2 ft-lbAverage value: 26.8 J Grade Count:4
Tensile Creep Modulus, 1 hour 1800 - 2200 MPa261000 - 319000 psiAverage value: 2080 MPa Grade Count:5
Tensile Creep Modulus, 1000 hours 1300 - 1800 MPa189000 - 261000 psiAverage value: 1630 MPa Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+18 ohm-cm100 - 1.00e+18 ohm-cmAverage value: 1.08e+17 ohm-cm Grade Count:109
Surface Resistance 100 - 1.50e+15 ohm100 - 1.50e+15 ohmAverage value: 3.29e+14 ohm Grade Count:91
Static Decay 0.0100 - 2.00 sec0.0100 - 2.00 secAverage value: 0.362 sec Grade Count:6
Dielectric Constant 2.00 - 3.002.00 - 3.00Average value: 2.46 Grade Count:101
Dielectric Strength 15.7 - 155 kV/mm400 - 3940 kV/inAverage value: 48.7 kV/mm Grade Count:121
Dissipation Factor 0.000100 - 0.001000.000100 - 0.00100Average value: 0.000365 Grade Count:54
Arc Resistance 60.0 - 180 sec60.0 - 180 secAverage value: 119 sec Grade Count:16
Comparative Tracking Index 250 - 600 V250 - 600 VAverage value: 454 V Grade Count:55
Hot Wire Ignition, HWI 7.00 - 60.0 sec7.00 - 60.0 secAverage value: 20.0 sec Grade Count:14
High Amp Arc Ignition, HAI 60.0 - 120 arcs60.0 - 120 arcsAverage value: 112 arcs Grade Count:14
High Voltage Arc-Tracking Rate, HVTR 10.0 - 80.0 mm/min0.394 - 3.15 in/minAverage value: 37.1 mm/min Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.20 - 100 µm/m-°C4.00 - 55.6 µin/in-°FAverage value: 80.6 µm/m-°C Grade Count:138
Specific Heat Capacity 1.79 - 2.20 J/g-°C0.428 - 0.526 BTU/lb-°FAverage value: 2.06 J/g-°C Grade Count:5
Thermal Conductivity 0.134 - 0.188 W/m-K0.930 - 1.30 BTU-in/hr-ft²-°FAverage value: 0.169 W/m-K Grade Count:27
Maximum Service Temperature, Air 80.0 - 97.8 °C176 - 208 °FAverage value: 91.6 °C Grade Count:15
Hot Ball Pressure Test 75.0 - 80.0 °C167 - 176 °FAverage value: 78.3 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 104 °C140 - 220 °FAverage value: 87.4 °C Grade Count:129
Deflection Temperature at 1.8 MPa (264 psi) 31.1 - 137 °C88.0 - 279 °FAverage value: 81.9 °C Grade Count:383
Vicat Softening Point 35.0 - 113 °C95.0 - 235 °FAverage value: 95.6 °C Grade Count:439
Heat Distortion Temperature 77.2 - 93.9 °C171 - 201 °FAverage value: 87.0 °C Grade Count:11
UL RTI, Electrical 50.0 °C122 °FAverage value: 50.0 °C Grade Count:8
UL RTI, Mechanical with Impact 50.0 °C122 °FAverage value: 50.0 °C Grade Count:8
UL RTI, Mechanical without Impact 50.0 °C122 °FAverage value: 50.0 °C Grade Count:8
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:311
Flame Spread 28.0 - 34.0 mm/min1.10 - 1.34 in/minAverage value: 29.3 mm/min Grade Count:6
Oxygen Index 18.0 %18.0 %Average value: 18.0 % Grade Count:19
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 707 °C Grade Count:19
 
Optical PropertiesMetricEnglishComments
Haze 1.00 - 30.0 %1.00 - 30.0 %Average value: 5.47 % Grade Count:12
Gloss 9.00 - 98.0 %9.00 - 98.0 %Average value: 67.4 % Grade Count:103
Transmission, Visible 82.0 - 89.0 %82.0 - 89.0 %Average value: 86.6 % Grade Count:11
 
Processing PropertiesMetricEnglishComments
Processing Temperature 95.6 - 280 °C204 - 536 °FAverage value: 210 °C Grade Count:38
Nozzle Temperature 188 - 260 °C370 - 500 °FAverage value: 221 °C Grade Count:26
Die Temperature 199 - 232 °C390 - 450 °FAverage value: 216 °C Grade Count:8
Melt Temperature 80.0 - 300 °C176 - 572 °FAverage value: 217 °C Grade Count:182
Mold Temperature 4.00 - 100 °C39.2 - 212 °FAverage value: 49.2 °C Grade Count:150
Injection Velocity 200 mm/sec7.87 in/secAverage value: 200 mm/sec Grade Count:10
Drying Temperature 60.0 - 160 °C140 - 320 °FAverage value: 79.4 °C Grade Count:54
Moisture Content 0.100 - 0.250 %0.100 - 0.250 %Average value: 0.194 % Grade Count:8
Injection Pressure 2.76 - 137 MPa400 - 19900 psiAverage value: 77.7 MPa Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene, Molded, Unreinforced
Overview of materials for Expanded Polystyrene (EPS)
Overview of materials for Polypropylene, Molded
Overview of materials for Polystyrene, Transparent Grade
Overview of materials for Polystyrene, Extrusion Grade

O4802 / 78412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.