MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Elvacite® 2043 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 2043 is a low molecular weight ethyl methacrylate copolymer. It is a fast – dissolving, low viscosity resin with alcohol solubility for flexographic inks. Most compatible grade. It provides excellent pigment wetting ability and broad solubility for use in lacquers for solvent – sensitive substrates.

Information provided by Lucite International

Key Words: Methyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/cc
Particle Size 140 - 220 µm140 - 220 µm
Viscosity Measurement 0.18 - 0.2380.18 - 0.238Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 50000 g/mol50000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 8.08.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 1111Tukon Hardness
Tensile Strength 6.89 MPa999 psi
Elongation at Break 0.60 %0.60 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 66.0 °C151 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.60 %0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Elvacite® 2013 Acrylic Resin
Lucite International Elvacite® 2045 Acrylic Resin
Lucite International Elvacite® 2044 Acrylic Resin
Lucite International Elvacite® 2042 Acrylic Resin
Lucite International Elvacite® 2016 Acrylic Resin

PLUCIT9460 / 150174

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.