MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Elvacite® 2013 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 2013 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. It is a fast – dissolving, low viscosity grade with quick solvent release for use in industrial lacquers, aerosols, inks, and coatings for plastics. Elvacite® 2013 is softer than the methyl methacrylate grades.

Applications: aerosols, industrial lacquers, inks, coatings

Information provided by Lucite International

Key Words: Methyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Particle Size 160 - 200 µm160 - 200 µm
Viscosity Measurement 0.156 - 0.1740.156 - 0.174Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 34000 g/mol34000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 5.05.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 1313Tukon Hardness
Tensile Strength 11.0 MPa1600 psi
Elongation at Break 0.50 %0.50 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 76.0 °C169 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.35 %0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Elvacite® 2043 Acrylic Resin
Lucite International Elvacite® 2045 Acrylic Resin
Lucite International Elvacite® 2044 Acrylic Resin
Lucite International Elvacite® 2016 Acrylic Resin
Lucite International Elvacite® 2014 Acrylic Resin

PLUCIT9452 / 150166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.