MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell AClyn® 201 EAA copolymer
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid; Ionomer

Material Notes: A calcium ionomer of an EAA copolymer. Used as a pigment dispersing agent for masterbatches in polar resin systems due to enhanced compatibility with the resin carrier.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 5500 cP
@Temperature 190 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 42
 
Thermal PropertiesOriginal ValueComments
Dropping Point 102 °CMettler
 
Descriptive Properties
Product FormPastille

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell A-C® 5180 EAA copolymer
Honeywell A-C® 5120 EAA copolymer
Honeywell AClyn® 201A EAA copolymer
Honeywell A-C® 580 EAA copolymer
Honeywell AClyn® 246 EAA copolymer

PHONWL084 / 179629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.