MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODUR® MGQ32135 + BAYTEC® D13 + BAYTEC® XL B (Catalyst SD6-40 or SD6-160), 80 A Polyurethane, MDI-PPG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccBAYTEC® XL B
 1.10 g/ccDESMODUR® MGQ32135
 1.14 g/ccBAYTEC® D13
 1.18 g/cc
Viscosity 30 cPBAYTEC® XL B
 390 cPBAYTEC® D13
 400 cPDESMODUR® MGQ32135
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80DIN 53505
 77
@Temperature 80.0 °C
DIN 53505
 87
@Temperature -5.00 °C
DIN 53505
Tensile Strength at Break 47.0 MPaDIN 53504
Tensile Stress at Strain 1.80 MPa
@Strain 10 %
DIN 53504
Elongation at Break 575 %DIN 53504
100% Modulus 0.00560 GPa
@Strain 100 %
DIN 53504
200% Modulus 0.00840 GPa
@Strain 200 %
DIN 53504
300% Modulus 0.0115 GPa
@Strain 300 %
DIN 53504
Resilience 30[%]; DIN 53512
Tear Strength 200 pliwith nick; ISO 34-1
 525 pliwithout nick; ISO 34-1
Abrasion 20[mm3]; ISO 4649
Compression Set 46 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815-1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 45.0 °CDESMODUR® MGQ32135
 45.0 °CBAYTEC® XL B
 60.0 °CBAYTEC® D13
Mold Temperature 100 °C
Pot Life 2.167 minin a heated sheet mold
 3.75 min400g mixture in a non heat bot
 
Descriptive Properties
AppearanceliquidDESMODUR® MGQ32135
 solidBAYTEC® D13
 solidBAYTEC® XL B
Content10.4Parts by weight of BAYTEC® XL B
 100Parts by weight of prepolymer
 13.25-13.65%NCO
 45Parts by weight of BAYTEC® D13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Covestro MONDUR® TD 80 Grade B Polyurethane
Covestro MONDUR® TD 80 Grade A Polyurethane
Covestro DESMODUR® MLQ22165 + BAYTEC® L20 + BAYTEC® XL B (Catalyst SD11-2) 80 A Polyurethane, MDI- Caprolactone

PCOVEST0478 / 202261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.