MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro MONDUR® TD 80 Grade B Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Mondur TD 80 Grade B is an aromatic diisocyanate mixture of 2,4 and 2,6 toluene diisocyanate (TDI) isomers in the ratio of 80/20.

Properties / Applications: Mondur TD 80 Grade B diisocyanate (increased acidity) is used to prepare prepolymer resins which are subsequently formulated into coatings, adhesives and sealant systems. As with any product, use of Mondur TD 80 Grade B diisocyanate in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/cc
 
Thermal PropertiesMetricEnglishComments
Flash Point 127 °C261 °FPMCC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5661.566
 
Descriptive Properties
Acidity0.009-0.01%as HCl
AppearanceWater white to pale yellow liquid
Boling Point251°C
Color<25APHA
Content>99.7%Assay
 0.008-0.015%Hydrolyzable chlorides
 18.5-20.5%2,6-Isomer ratio
 79.5-81.5%2,4-Isomer ratio
Crystallization13°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Covestro MONDUR® TD 80 Grade A Polyurethane
Covestro DESMODUR® MLQ22165 + BAYTEC® L20 + BAYTEC® XL B (Catalyst SD11-2) 80 A Polyurethane, MDI- Caprolactone
Covestro DESMODUR® MGQ32135 + BAYTEC® D13 + BAYTEC® XL B (Catalyst SD6-40 or SD6-160), 80 A Polyurethane, MDI-PPG

PCOVEST0921 / 202704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.