MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
MetalTek MTEK 80-10-10 Cast UNS C93700 Bearing Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Popular alloy with score resistance, structural uniformity, shear properties, compressive strength and low cost.

Applications: Bearings, bushings, sleeves, liners, piston rings, hydraulic parts

Information provided by MetalTek

Cast UNS C93700; Cast Grade C93700; Cast ASTM B271, B22, B584; SAE 64 (Discontinued); Mil QQ-C-390B

Key Words: High Lead Tin Bronze
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.95 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 70500 kg
Tensile Strength, Ultimate >= 205 MPa
Tensile Strength, Yield >= 80.0 MPa
Elongation at Break >= 15 %
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 80 %
Lead, Pb 10 %
Tin, Sn 10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93700, Copper Casting Alloy (SAE 64)
MetalTek MTEK 83-7-7-3 Cast UNS C93200 Bearing Bronze
MetalTek MTEK 78-7-15 HI LEAD Cast UNS C93800 Bearing Bronze
MetalTek MTEK 85-5-5-5 Cast UNS C83600 Bearing Bronze
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660

NMETEK020 / 18270

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.