MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Northstar Polymers MPS-M23B Room-Temperature Curable Microcellular Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: This foam polyurethane formulation is designed to yield closed-cell microcellular foam by either hand-mixing or machine casting method at room temperature. The components are liquid at room temperature. It is designed to be used in compression molding process with 10% or higher compression rate. For a small quantity, this can be batched manually by hand tools. This can also be cast with a multi-component meter-mixing/dispensing machine. The free-rise density of the foam is 23 pounds-per-cubic-foot.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 90.0 °FPrepolymer Temperature
 70.0 - 90.0 °FCuring Agent Temperature
Mold Temperature 100 - 120 °F
Cure Time 0.250 hour
@Temperature 43.3 °C
De-mold Time
 48.0 hour
@Temperature 25.0 °C
Complete Cure Cycle
Pot Life 0.750 min
 
Descriptive Properties
Curing AgentPBD-025
Mixing Time10minimum for mixing by hand
PrepolymerMSA-018
Weight Ratio1:1.762Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Synfoam® LG-20 Syntactic Foam
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam
General Plastics LAST-A-FOAM® R-9340 Thermal Isolation Blocks
Dow TONE™ 305 Polyol

PNORTH884 / 162600

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.