MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Synfoam® LG-20 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Castable. SynFoam LG is a unique, expandable, closed cell syntactic foam that provides very low density and moderate strength. SynFoam LG is an ideal replacement for polyurethane foams where higher modulus is needed to support lightweight structures. It is suitable for numerous marine and aerospace applications or where machining of parts is either impractical or too expensive. SynFoam LG is available as 1, 2, and 5 gallon kits. Each kit contains an A and B side that must be mixed together prior to casting. Cure is achieved within 24 hours and full properties will be realized after 7 days at room temperature. Densities can be customized to the user's specifications. Interlayer adhesion allowing large structures to be made with multiple pours.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.288 - 0.352 g/cc0.0104 - 0.0127 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 10.3 MPa1500 psi
Compressive Modulus 0.345 GPa50.0 ksi
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 95.0 °C203 °F
 
Descriptive Properties
Depth Rating (m)460

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam
J6 Polymers JFOAM™ S-1200 Engineered Specialty Foam
General Plastics LAST-A-FOAM® R-9340 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® FR-7108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3840 FST Polyurethane Foam

PSYNF039 / 192914

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.