MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Conventus Polymers Duraflex TPC-ET55 NAT Polyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Duraflex TPC-ET55 NAT is a general purpose flexible polyester elastomer. It offers a unique combination of mechanical, physical, and chemical properties for high performance applications. It offers very high impact strength and flexibility at low temperatures, excellent fatigue resistance, excellent oil & solvent resistance, and is easy to process.

Information provided by Conventus Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.70 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.00011 - 0.00015 in/in
@Thickness 3.20 mm
ASTM D955
Melt Flow 25 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 54ASTM D2240
Tensile Strength at Break 4980 psi
@Thickness 2.00 mm
ASTM D638
Elongation at Break 500 %
@Thickness 2.00 mm
ASTM D638
Izod Impact, Notched 2.80 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 NB
@Temperature 22.8 °C
ASTM D256
Tear Strength 840 pliASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 401 °FASTM D3418
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 428 - 464 °F
Zone 1 392 - 428 °F
Zone 2 410 - 446 °F
Zone 3 428 - 464 °F
Melt Temperature 392 - 464 °F
Mold Temperature 68.0 - 104 °F
Drying Temperature 176 - 194 °F
@Time 10800 - 14400 sec
Moisture Content <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Conventus Polymers Duraflex TPC-ET33 NAT Polyester TPE
Celanese Riteflex® 647 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)
Celanese Hytrel® 5556 TPC-ET

PCONV941 / 233859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.