MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Conventus Polymers Duraflex TPC-ET55 NAT Polyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Duraflex TPC-ET55 NAT is a general purpose flexible polyester elastomer. It offers a unique combination of mechanical, physical, and chemical properties for high performance applications. It offers very high impact strength and flexibility at low temperatures, excellent fatigue resistance, excellent oil & solvent resistance, and is easy to process.

Information provided by Conventus Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00011 - 0.00015 cm/cm
@Thickness 3.20 mm
0.00011 - 0.00015 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 25 g/10 min25 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454ASTM D2240
Tensile Strength at Break 34.3 MPa
@Thickness 2.00 mm
4980 psi
@Thickness 0.0787 in
ASTM D638
Elongation at Break 500 %
@Thickness 2.00 mm
500 %
@Thickness 0.0787 in
ASTM D638
Izod Impact, Notched  1.49 J/cm
@Temperature -40.0 °C
2.80 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ASTM D256
Tear Strength 147 kN/m840 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Melting Point 205 °C401 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 240 °C428 - 464 °F
Zone 1 200 - 220 °C392 - 428 °F
Zone 2 210 - 230 °C410 - 446 °F
Zone 3 220 - 240 °C428 - 464 °F
Melt Temperature 200 - 240 °C392 - 464 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 - 90.0 °C
@Time 10800 - 14400 sec
176 - 194 °F
@Time 3.00 - 4.00 hour
Moisture Content <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Conventus Polymers Duraflex TPC-ET33 NAT Polyester TPE
Celanese Riteflex® 647 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)
Celanese Hytrel® 5556 TPC-ET

PCONV941 / 233859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.