MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® MO Polyester Film, 500 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® MO polyester film has excellent electrical properties. This film offer exceptional cut-through resistance, low shrinkage, low moisture absorption, and high thermal durability. Mylar® MO film is used as insulation in systems that have been given Class B ratings by Underwriters Laboratories (UL). It offers product uniformity that enhances processing on automatic slot and wedge insertion equipment.

The inherit mechanical durability of Mylar® Type MO film and its good dielectric and thermal durability characteristics give this film multiple advantages in motors and generators.

Typical Applications: Mylar® MO film is being widely used for electrical insulation in slot liners, wedges, and phase insulation for motors and generators. This film is also frequently used in hermetic motor/compressor sealed units, fractional horse power motors, diaphragms, and industrial laminations.

Approvals: UL 94 VTM-2 - for 500 gauge ( 0.13 mm only)

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.3923 g/cc
Thickness 5.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 140 %ASTM D882A
Film Elongation at Break, TD 115 %ASTM D882A
Film Tensile Strength at Break, MD 27000 psiASTM D882A
Film Tensile Strength at Break, TD 30000 psiASTM D882A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 2700 V/mil1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 13500 V1/4" electrode 500 V/sec 25°C in air; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
Shrinkage, MD 1.1 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.70 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.64 - 1.67typical of Mylar®
Optical Density 14
 
Descriptive Properties
Yield (nominal)4000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Extruded
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
DuPont Teijin Films Mylar® M813 Polyester Film, 48 Gauge

PDTZ9377 / 139697

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.