MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® M813 Polyester Film, 48 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® M813 is a clear, pretreated base film with high gloss, low haze, and excellent processability. It is a one side pre-treated polyester designed for improved ink adhesion and may be suitable for use in medical applications.

General Product Info: Mylar® M813 film provides good clarity for reverse printing and allows inks to shine through with high quality. The film's pretreated surface also provides improved adhesion for various coatings and adhesives, often eliminating the need for any type of priming operation. The chemical pretreatment on Mylar® M813 film does not result in a performance or shelf life decline over time, and generally is superior to corona treated film. Mylar® M813 film features good clarity and handling characteristics in metallizing operations. When aluminum metallized, the film exhibits excellent aesthetic quality as well as the best barrier to oxygen and moisture in a flexible packaging film. Polyester is more thermally stable at higher temperatures and has higher tensile strength than materials such as polypropylene or polyethylene. Mylar® polyester film also maintains an excellent film thickness profile and roll formation to ensure consistent processability in the operations. These characteristics are particularly important in complex, multi-stage printing operations where holding print register is critical to print quality. As print complexity, quality and speeds increase, Mylar® film provides a cost-effective solution for the packaging industry.

Approvals: FDA Food Contact Status - All gauges of Mylar® M813 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers, Sections (f) and (g). This regulation describes films which may be safely used in contact with all types of food, excluding alcoholic beverages, at temperatures not to exceed 250°F. Drug Master File - This product is listed in our Drug Master File.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Water Vapor Transmission  0.776 g/m²/day
@Temperature 38.0 °C
0.0500 g/100 in²/day
@Temperature 100 °F
90% RH, metallized; ASTM F1249
 31.0 g/m²/day
@Temperature 38.0 °C
2.00 g/100 in²/day
@Temperature 100 °F
90% RH, unmetallized; ASTM F1249
Thickness 12.2 microns0.480 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 110 %110 %ASTM D882A
Film Elongation at Break, TD 70 %70 %ASTM D882A
Coefficient of Friction, Dynamic 0.400.40A-B; ASTM D1894
Coefficient of Friction, Static 0.500.50ASTM D1894
Film Tensile Strength at Break, MD 214 MPa31000 psiASTM D882A
Film Tensile Strength at Break, TD 290 MPa42000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Maximum Service Temperature, Air 121 °C250 °F
Shrinkage, MD 3.5 %
@Temperature 190 °C,
Time 300 sec
3.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 3.5 %
@Temperature 190 °C,
Time 300 sec
3.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.64 - 1.671.64 - 1.67typical of Mylar®
Haze 3.6 %3.6 %ASTM D1003
Transmission, Visible 88.5 %88.5 %ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)0.08 cc/100 in2O2, 24 hr; ASTM D1434 77°F/75% RH/1 ATM (metallized)
 1.6 cc/100 in2Nitrogen; ASTM D1434 (24 hrs @ 77°F and 75% RH @ 1 ATM)
 31 cc/100 in2Carbon Dioxide; ASTM D1434 (24 hrs @ 77°F and 75% RH @ 1 ATM)
 6 cc/100 in2O2, 24 hr; ASTM D1434 (unmetallized)
Yield (nominal)42200 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® MLBT Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® MO Polyester Film, 500 Gauge

PDTZ9360 / 139680

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.