MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GY-70 (Celanese) Carbon Fiber  (discontinued **)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: Polyacrylonitrile fibers are converted into carbon fibers through oxidation in air between 200 - 300°C, followed by carbonization and then graphitization in inert atmospheres at temperatures up to 3000°C.

Information provided by Celanese Corporation.

Key Words: composites, fibers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2000 MPaFiber only. Composites containing this fiber may have tensile strength of 750 MPa.
Modulus of Elasticity 300 GPaor 500 GPa for fiber
Shear Strength 50.0 MPaInterlaminar shear.

References for this datasheet.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Solvay CYCOM® 381 Epoxy Prepreg with IM7 Uni-graphite and 148FAW Epoxy
Hexcel® HexTow® IM6 Carbon Fiber - Epoxy Composite
Poco Graphite DFP-3-2 Ion Implant Grade Graphite
Poco Graphite Fabmate® Pore-Free Specialty Graphite

PCO003 / 28594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.