MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite Fabmate® Pore-Free Specialty Graphite  (discontinued **)
Categories: Carbon; Graphite

Material Notes: Shore scleroscope C-2 hardness is 77. FABMATE is the trade name for a high-strength, finished product that has been purified, machined and subjected to Poco Graphite's proprietary carbon modification treatment.

FABMATE products are designed for use in clean rooms. They are ideal for semiconductor applications requiring exceptional cleanliness and a pore-free surface.

The graphite substrate is fine-grained, high strength graphite that has excellent machinability. After machining, the surface can be textured if the end product is to be used in thin film deposition. The graphite is next purified and given an amorphous carbon treatment. This treatment is unique because it does more than coat the surface. It also infiltrates and locks onto the graphite. This treatment provides a hard, abrasion resistant surface that produces no particles. The result is a surface that is grain free, harder than the substrate, but extremely thin.

This nonporous surface does not allow absorption of acids. FABMATE resists attack by hydrofluoric (HF) and most other acids used in the cleaning process.

Information provided by Poco Graphite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.82 g/cc0.0658 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 69.0 MPa10000 psi
Flexural Strength 89.6 MPa13000 psi
Compressive Yield Strength 152 MPa22000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00135 ohm-cm0.00135 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.40 µm/m-°C
@Temperature 20.0 - 1000 °C
4.67 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 10.0 W/m-K69.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 510 °C950 °FOxidation threshold
Maximum Service Temperature, Inert 2500 °C4530 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 100 %100 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite DFP-3-2 Ion Implant Grade Graphite
Carlisle 201HD Carbon-Carbon Composite
GY-70 (Celanese) Carbon Fiber
Solvay CYCOM® 381 Epoxy Prepreg with IM7 Uni-graphite and 148FAW Epoxy
Graphite, Carbon, C

EPOC09 / 5676

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.