MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Cookson Group Plaskon® 3400F-14 Conventional Encapsulant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: This material is a fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs and medium lead count QFPs. It was developed with fine filler particles especially for use with automated or conventional molding equipment and offers a balance of end use properties.

Features

  • Excellent moldability
  • Superior cosmetics
  • Improved markability
  • Fast cycle times

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc
Viscosity 1000 - 1600 cP
@Temperature 175 °C
1000 - 1600 cP
@Temperature 347 °F
Automatic orifice Viscosity
Spiral Flow 54.0 - 78.0 cm21.3 - 30.7 inat 177°C and 1000 psi
Ash 71.4 %71.4 %
Storage Temperature <= 5.00 °C<= 41.0 °FRecommended
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070Cull hot, 90 sec @ 175°C
Flexural Strength 124.1 MPa17990 psi
Flexural Modulus 15.17 GPa2200 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.58e+16 ohm-cm1.58e+16 ohm-cm
Dielectric Constant 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
Dielectric Strength >= 15.7 kV/mm>= 400 kV/in
Dissipation Factor 0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
Arc Resistance 180 sec180 sec110V AC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.0 µm/m-°C
@Temperature 20.0 °C
11.7 µin/in-°F
@Temperature 68.0 °F
Alpha 1
 60.0 µm/m-°C
@Temperature 20.0 °C
33.3 µin/in-°F
@Temperature 68.0 °F
Alpha 2
Thermal Conductivity 0.669 W/m-K4.64 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 150 °C302 °F
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Oxygen Index 32 %32 %
 
Processing PropertiesMetricEnglishComments
Mold Temperature 170 - 185 °C338 - 365 °F
Back Pressure 5.17 - 6.89 MPa750 - 1000 psi
Cure Time  0.333 - 0.433 min
@Temperature 177 °C
0.00556 - 0.00722 hour
@Temperature 351 °F
 240 - 720 min
@Temperature 175 °C
4.00 - 12.0 hour
@Temperature 347 °F
Post mold
Gel Time 0.133 min0.133 minRam follower, at 177°C
Shelf Life 0.0670 Month0.0670 Monthat 35°C, <40% loss of spiral flow
 0.167 Month0.167 Monthat 21°C, <40% loss of spiral flow
 24.0 Month24.0 Monthat 5°C, <40% loss of spiral flow
 
Descriptive Properties
Hydrolyzable Cl<10 ppm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLASK028 / 56318

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.