Description: NBR 7150 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 7150 is a non staining, medium mooney, medium low acrylonitrile polymer designed to aid in processing operations such as transfer and compression molding. NBR 7150 offers good balance of oil and fuel resistance in low temperature and is no need for additional fatty acid for sulfur cure system activation. Applications: NBR 7150 is recommended to use in industrial and automotive parts such as oil hose. CAS No: 9003-18-3 Information provided by LG Chemical |