MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Trelleborg Sealing Solutions HiMod® 911 Thermoplastic Bearing
Categories: Polymer; Thermoplastic

Material Notes: Thermoplastic Bearing

Characteristics: HiMod® 911 is an excellent self lubricating, maintenance free, long wearing bearing material that operates with very low friction. HiMod® 911 is ideal for applications with intermittent temperatures of 200°F. It performs under conditions where moderate loads and speeds exist.

Applications: Office machines, home appliances, computer equipment, ski lifts, lumber mill equipment, farm equipment, exercise equipment, bicycles, conveyors, packaging equipment, food processing equipment, golf carts.

Information provided by Busak + Shamban, now Trelleborg Sealing Solutions.

Busak+Shamban changed its name to Trelleborg Sealing Solutions in 2007.

Key Words: Busak + Shamban; TI Group; Smiths Group
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Limiting Pressure Velocity 0.260 MPa-m/sec7420 psi-ft/min
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °FContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy 400
Trelleborg Sealing Solutions Turcite® TA Self-Lubricating Thermoplastic Rod
Special Metals MONEL® Alloy R-405
Special Metals MONEL® Alloy K-500
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod

PSMIT5 / 67855

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.