MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epsan Eplamid 6 GV0 20 NC Q1C0C001 Polyamide 6, Halogenated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant polyamide 6 reinforced with 20% of glass fiber, heat stabilized for injection molding. Halogenated flame retardant grade, compliance with RoHs derivatives, with rating UL94 V0 and glow-wire at 960°C, combines excellent all around mechanical properties.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cmParallel; ISO 294-4
 0.0070 cm/cmNormal; ISO 294-4
Ash 20 %ISO 3451-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 130 MPaISO 527-2
Elongation at Break 3.0 %ISO 527-2
Tensile Modulus 7600 MPaISO 527-2
Flexural Strength 210 MPaISO 178
Flexural Modulus 7200 MPaISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180/1A
Charpy Impact, Notched 9.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 VEN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 3146
Flammability, UL94 V-0
@Thickness 0.800 mm
EN 60695-11-10
Glow Wire Ignition Temperature 750 °C
@Thickness 0.800 mm
EN 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 °CRecommended Injection Molding Temperature
Drying Temperature 80.0 °CAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epsan Eplamid 6 GX0 20 NC Q1C0B601 Polyamide 6, Halogen Free
Epsan Eplamid 6 NC HV A3,6 Polyamide 6
Epsan Eplamid 66 GFI 20 NC Q1C0A801 Polyamide 66
Epsan Eplamid 6 CBR 15 NC Q1B501 Polyamide 6
Epsan Eplamid 6 BK Q101 Polyamide 6

PEPSAN030 / 186344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.