MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Eplamid 6 GX0 20 NC Q1C0B601 Polyamide 6, Halogen Free
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant polyamide 6 reinforced with 20% glass fiber, heat stabilized for injection molding. Halogen and red phosphorous free flame retardant grade, compliance with RoHs derivatives, with rating UL94 V0 and glow-wire at 960°C, combines excellent all around mechanical properties.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inParallel; ISO 294-4
 0.0080 cm/cm0.0080 in/inNormal; ISO 294-4
Ash 20 %20 %ISO 3451-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 90.0 MPa13100 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 5.80 GPa841 ksiISO 527-2
Flexural Strength 150 MPa21800 psiISO 178
Flexural Modulus 5.50 GPa798 ksiISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
EN 60695-11-10
Glow Wire Ignition Temperature 750 °C
@Thickness 0.800 mm
1380 °F
@Thickness 0.0315 in
EN 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30
Envalior Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Epsan Eplamid 6 GV0 20 NC Q1C0C001 Polyamide 6, Halogenated
Epsan Eplamid 6 NC HV A3,6 Polyamide 6
Epsan Eplamid 66 GFI 20 NC Q1C0A801 Polyamide 66

PEPSAN027 / 186341

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.