MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ASTM A529 Steel
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Copper content of 0.20% is a minimum when copper steel is specified. For plates wider than 610 mm, the tests were taken in the transverse direction and the elongation requirement is reduced by 2%. The following are suggested consumables for arc welding processes: For 0.476 - 1.27 cm (3/16 - 1/2 in.) thicknesses - Manual Shielded Metal-Arc (AWS A5.5) Low Hydrogen Electrodes E60xx, and E70xx; Submerged Arc (AWS A5.23) F6x-Exxx, and F7x-Exxx; Gas Metal-Arc (AWS A5.28) ER70S-x; Flux Cored-Arc (AWS A5.29) E6xT-x, and E7xT-x except -2, -3, -10, or -GS.

Key Words: copper-steels, copper steels, UNS K02703
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 415 - 585 MPa
Tensile Strength, Yield 290 MPa
Elongation at Break 19 %in 200mm
Bulk Modulus 160 GPaTypical for steel
Shear Modulus 80.0 GPaTypical for steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.27 %
Copper, Cu >= 0.20 %
Iron, Fe 98 %
Manganese, Mn <= 1.2 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A36 Steel, plate
ASTM A572 Steel, grade 50
Bethlehem Steel ASTM A529 Grade 50 3/16 to 1 in. thick, as-rolled steel plate
Bethlehem Steel ASTM A529 Grade 42 3/16 to 1/2 in. thick, as-rolled steel plate
ASTM A36 Steel, bar

MS529A / 13982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.