MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Petra® 7010 WT 7729 15% Glass Filled PET
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes: Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface aesthetics, it exhibits excellent melt stability and high flow over a broad range of processing conditions. The combination of high strength and dimensional stability enable its use in structural applications designed for metal.

Application: Petra 7010 WT7729 is recommended for applications such as appliance door handles and knobs.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527
Elongation at Break 1.5 %ISO 527
Flexural Modulus 6800 MPaISO 178
Charpy Impact Unnotched 15.0 kJ/m²
@Temperature 5.00 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 245 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 100 - 110 °C
Dry Time 2 - 4 hour
Moisture Content 0.20 %
 
Descriptive Properties
ColorWT 7792
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Petra® 7010 BK 5830 15% Glass Filled PET
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
BASF Petra® 130 30% Glass Filled PET
BASF Petra® 110 BK-112 15% Glass Filled PET
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET

PBASG0553 / 132186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.