MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Petra® 110 BK-112 15% Glass Filled PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes: Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength and stiffness at elevated temperatures with good chemical resistance and dimensional stability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 105 MPa15200 psi5mm/min; ISO 527
Elongation at Break 3.5 %3.5 %5mm/min; ISO 527
 3.5 %3.5 %0.2 in/min; ASTM Test
Tensile Modulus 6.68 GPa969 ksi1mm/min; ISO 527
Flexural Strength 145 MPa21000 psiASTM Test
Flexural Modulus 5.35 GPa776 ksiASTM Test
 5.48 GPa795 ksiISO Data
Izod Impact, Notched 0.650 J/cm
@Thickness 3.17 mm
1.22 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO Test
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
IEC 60250
Dielectric Strength 36.0 kV/mm914 kV/inIEC 60243-1
Dissipation Factor  0.010
@Frequency 100 Hz
0.010
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C17.8 µin/in-°FISO 11359
CTE, linear, Transverse to Flow 79.0 µm/m-°C43.9 µin/in-°FISO 11359
Melting Point 245 °C473 °F10 K/min
 245 °C473 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 231 °C448 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 192 °C378 °FISO 75
 208 °C406 °FASTM Test
Flammability, UL94  HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 115 °C239 °FInjection molding
 
Descriptive Properties
ColorBK-112
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Petra® 7010 BK 5830 15% Glass Filled PET
BASF Petra® 130 30% Glass Filled PET
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
BASF Petra® 7010 WT 7729 15% Glass Filled PET
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET

PBASF9015 / 84779

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.