MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Armstrong A-2/H20 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Activators W or H-20 has a very low thermal expansion coefficient, especially important for bonding ceramics, porcelain, etc. A-2 with Activator A is qualified under Mil. Spec. MIL-A-47284 (MI).

Information provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 15000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84
Tensile Strength, Ultimate 5000 psiafter optimum cure
Elongation at Break 1.9 %
Adhesive Bond Strength 6450 psiSteel-Steel; after optimum cure
 1000 psi
@Temperature 82.2 °C
Aluminum-Aluminum tensile shear
 1500 psi
@Temperature -54.4 °C
Aluminum-Aluminum tensile shear
 1750 psi
@Temperature 25.0 °C
Aluminum-Aluminum tensile shear
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°C
@Temperature 20.0 °C
Glass Transition Temp, Tg 58.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 72.0 °F
 200 °FOptimum cure is 30 min. @ 200°F
 200 °FFast cure is 10 min. @ 200°F
Pot Life <= 90.0 min
@Temperature 25.0 °C
100 g
 
Descriptive Properties
ColorWhite
Mix Ratio10/1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Armstrong A-12 Epoxy Adhesive, at 1:1 Mix Ratio
Atom Adhesives AA-BOND F110 Epoxy Adhesive
Overview of materials for Epoxy Adhesive
Abatron AboCast/AboCure 8502-1 Epoxy

PARM05 / 24537

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.