MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Buckeye Polymers BP RPP 1012 T BLK Polypropylene, Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes: Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents. Buckeye Polymers can also customize these materials through the addition of UV packages, custom color matching, and processing additives.

    Product Features:
  • Increased stiffness and heat deflection
  • Good UV resistance
  • Industrial, appliance, construction markets
  • Good scratch and mar resistance
  • Appearance: Black

    Forms: Pellets

    Processing Method: Injection Molding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage 0.012 - 0.014 in/inASTM D955
Melt Flow 8.0 - 12 g/10 minASTM D1238
Ash 8.0 - 12 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 2910 psiASTM D638
Flexural Modulus >= 155000 psiASTM D790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Renol PPT10 Polypropylene Copolymer, Talc Filled
LyondellBasell Hifax 5519/1 G 1750 Polypropylene, 10% Talc Filled
Formosa Plastics Formolene® 4100N Injection Molding Polypropylene
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade

PBUCK027 / 104494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.