MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Novolen® 1100 L Polypropylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Injection molded parts, film tape, fibrillated film and monofilaments.

Data was collected by ISO methods and provided by BASF.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
Water Absorption 0.10 %0.10 %
Moisture Absorption at Equilibrium 0.10 %0.10 %
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/in
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 10 %10 %
Tensile Modulus 1.50 GPa218 ksi
Charpy Impact Unnotched 14.0 J/cm²66.6 ft-lb/in²
 1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²
 0.150 J/cm²
@Temperature -30.0 °C
0.714 ft-lb/in²
@Temperature -22.0 °F
Tensile Creep Modulus, 1 hour 700 MPa102000 psi
Tensile Creep Modulus, 1000 hours 380 MPa55100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.3
@Frequency 100 Hz
2.3
@Frequency 100 Hz
 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
Dielectric Strength 140 kV/mm3560 kV/in
Dissipation Factor  0.000070
@Frequency 100 Hz
0.000070
@Frequency 100 Hz
 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 135 µm/m-°C
@Temperature 20.0 °C
75.0 µin/in-°F
@Temperature 68.0 °F
Melting Point 163 °C325 °F
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °F
Vicat Softening Point 92.0 °C198 °F
Flammability, UL94 HB
@Thickness 3.18 mm
HB
@Thickness 0.125 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade

PSF123 / 66704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.