MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lanxess X_Butyl™ R 1551 PG Butyl Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: X_Butyl™ R 1551 PG is a new low unsaturation, high purity regular butyl elastomer grade with improved cure characteristics. In resin cure systems, compounds containing new X_Butyl™ R 1551 PG achieve comparable crosslink density more quickly than existing regular butyl grades with higher unsaturation. The reduced unsaturation results in improved aging characteristics in resin cure applications such as curing bladders and envelopes while still offering improved production throughput.

Key Properties: In addition to the key properties of butyl rubber such as impermeability, X_Butyl™ R 1551 PG has:

  • improved purity (as measured by ash)
  • reduced additives
  • reduced unsaturation
  • improved cure characteristics
Benefits:
  • reduced cycle times for curing leading to higher production throughput
  • reduced curatives for resin cured articles
  • improved aging characteristics for a longer lasting product

      Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.30 %
Mooney Viscosity 46 - 56
@Temperature 125 °C
(1+8)
Ash <= 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 14.1 MPawith optimized cure package
 7.90 MPa
@Treatment Temp. 180 °C,
Time 173000 sec
Aged, with optimized cure package
Elongation at Break 749 %with optimized cure package
 271 %
@Treatment Temp. 180 °C,
Time 173000 sec
Aged, with optimized cure package
100% Modulus 0.00410 GPa
@Temperature 180 °C,
Time 173000 sec
Aged, with optimized cure package
 0.00180 GPa
@Strain 100 %
with optimized cure package
 
Descriptive Properties
Content>0.03%Antioxidant (non-staining)
 1.3-1.7 mol%Unsaturation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess X_Butyl™ BB 2040 Butyl Rubber
Lanxess X_Butyl™ I4565P Butyl Rubber
Lanxess X_Butyl™ R 0933 PG Butyl Rubber
Lanxess X_Butyl™ RB 402 Butyl Rubber
Sibur BK-1675S Butyl Rubber (IIR)

PLANY8649 / 209042

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.