MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 954-3 Curing Cyanate Resin, G80-600 Fiber
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  39.0 MPa
@Temperature 23.0 °C
5660 psi
@Temperature 73.4 °F
90°
 2227 MPa
@Temperature 23.0 °C
323000 psi
@Temperature 73.4 °F
Tensile Modulus  5.50 GPa
@Temperature 23.0 °C
798 ksi
@Temperature 73.4 °F
90°
 303 GPa
@Temperature 23.0 °C
43900 ksi
@Temperature 73.4 °F
Compressive Yield Strength 903 MPa
@Temperature 23.0 °C
131000 psi
@Temperature 73.4 °F
Compressive Modulus 296 GPa
@Temperature 23.0 °C
42900 ksi
@Temperature 73.4 °F
Shear Strength 72.0 MPa
@Temperature 22.0 °C
10400 psi
@Temperature 71.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Hexcel® HexPly® 954-3 Curing Cyanate Resin
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber
Hexcel® HexPly® 954-2A Curing Cyanate Resin, K1100 Fiber

PHEXC026 / 98496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.