Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength, Yield | 648 MPa @Temperature 23.0 °C | 94000 psi @Temperature 73.4 °F |
Elongation at Yield | 3.5 % @Temperature 23.0 °C | 3.5 % @Temperature 73.4 °F |
Tensile Modulus | 22.1 GPa @Temperature 23.0 °C | 3210 ksi @Temperature 73.4 °F |
Flexural Yield Strength | 765 MPa @Temperature 23.0 °C | 111000 psi @Temperature 73.4 °F |
Flexural Modulus | 20.7 GPa @Temperature 23.0 °C | 3000 ksi @Temperature 73.4 °F |
Compressive Yield Strength | 345 MPa @Temperature 163 °C | 50000 psi @Temperature 325 °F |
| 359 MPa @Temperature 149 °C | 52100 psi @Temperature 300 °F |
| 372 MPa @Temperature 177 °C | 54000 psi @Temperature 351 °F |
| 407 MPa @Temperature 163 °C | 59000 psi @Temperature 325 °F |
| 517 MPa @Temperature 23.0 °C | 75000 psi @Temperature 73.4 °F |
Compressive Modulus | 21.4 GPa @Temperature 177 °C | 3100 ksi @Temperature 351 °F |
| 23.4 GPa @Temperature 163 °C | 3390 ksi @Temperature 325 °F |
| 23.4 GPa @Temperature 149 °C | 3390 ksi @Temperature 300 °F |
| 23.4 GPa @Temperature 163 °C | 3390 ksi @Temperature 325 °F |
| 23.4 GPa @Temperature 23.0 °C | 3390 ksi @Temperature 73.4 °F |
Shear Strength | 37.2 MPa @Temperature 163 °C | 5400 psi @Temperature 325 °F |
| 44.1 MPa @Temperature 149 °C | 6400 psi @Temperature 300 °F |
| 44.8 MPa @Temperature 177 °C | 6500 psi @Temperature 351 °F |
| 46.2 MPa @Temperature 163 °C | 6700 psi @Temperature 325 °F |
| 71.7 MPa @Temperature 23.0 °C | 10400 psi @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Constant | 3.22 @Frequency 2.07e+10 Hz, Temperature 23.0 °C | 3.22 @Frequency 2.07e+10 Hz, Temperature 73.4 °F |
| 3.32 @Frequency 4.45e+10 Hz, Temperature 23.0 °C | 3.32 @Frequency 4.45e+10 Hz, Temperature 73.4 °F |
Dielectric Loss Index | 0.0060 @Frequency 2.07e+10 Hz, Temperature 23.0 °C | 0.0060 @Frequency 2.07e+10 Hz, Temperature 73.4 °F |
| 0.0060 @Frequency 4.45e+10 Hz, Temperature 23.0 °C | 0.0060 @Frequency 4.45e+10 Hz, Temperature 73.4 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.