MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resinoid 1312 Phenolic Molding, Glass Reinforced  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Data provided by the manufacturer.

The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/ccASTM D792A
Water Absorption 0.10 %24 hours R.T. ASTM D570
Linear Mold Shrinkage 0.0035 cm/cmPositive Mold; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 48.0 MPaASTM D651
Flexural Strength 84.0 MPaASTM D790
Flexural Modulus 14.0 GPaASTM D790
Compressive Strength 170 MPaASTM D695
Izod Impact, Notched 0.446 J/cmASTM D256A
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 - 399 V
@Thickness 3.05 mm
UL PLC 2 (250-399 V)
Hot Wire Ignition, HWI >= 120 sec
@Thickness 3.05 mm
UL PLC 0; UL PLC 0
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 3.05 mm
UL PLC 0; UL PLC 0
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
@Thickness 3.05 mm
UL PLC 0 (0-10 mm/min)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
UL RTI, Electrical 150 °C
UL RTI, Mechanical with Impact 150 °C
UL RTI, Mechanical without Impact 150 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Mold Temperature 155 - 180 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
Plenco 1500 Polyester, Granular, Compression Molded
Plenco PlasGlas™ 20118 High Strength Electrical 18% Glass Filled Thermoset Polyester BMC
Resinoid 2016 Phenolic Molding, Fabric Reinforced
A. Schulman Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC

PPHR00 / 56226

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.