MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 3499-3 X 102947 B Liquid Crystal Polymer (LCP), Thermally Conductive - Electrically Insulative
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.70 g/ccASTM D 792
Linear Mold Shrinkage 0.0040 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9000 psiASTM D 638
Elongation at Break 0.70 %ASTM D 638
Tensile Modulus 1800 ksiASTM D 638
Flexural Strength 13000 psiASTM D 790
Flexural Modulus 1850 ksiASTM D 790
Izod Impact, Notched 0.600 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 2.50 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cmASTM D 257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 9.55 µin/in-°FE 831
CTE, linear, Transverse to Flow 38.2 µin/in-°FE 831
Thermal Conductivity 11.1 BTU-in/hr-ft²-°FThrough-plane; E 1530
Deflection Temperature at 1.8 MPa (264 psi) 465 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 630 - 690 °F
Mold Temperature 150 - 250 °F
Drying Temperature 300 °F
Dry Time 8 hour
Dew Point -20.0 °F
Injection Pressure 12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
Kuraray Vectran® HT 1500/300 LCP Fiber
Celanese CoolPoly® D5502 Thermally Conductive Liquid Crystalline Polymer
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Epoxy Technology EPO-TEK® TZ101 Thermally Conductive Epoxy

PQZWA3225 / 91593

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.