MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.45 - 1.89 g/cc0.0524 - 0.0683 lb/in³Average value: 1.75 g/cc Grade Count:16
Filler Content 45.0 - 50.0 %45.0 - 50.0 %Average value: 45.7 % Grade Count:7
Water Absorption 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0575 % Grade Count:4
Moisture Absorption at Equilibrium 0.00600 - 1.10 %0.00600 - 1.10 %Average value: 0.372 % Grade Count:3
Linear Mold Shrinkage 0.000 - 0.00200 cm/cm0.000 - 0.00200 in/inAverage value: 0.000861 cm/cm Grade Count:14
Linear Mold Shrinkage, Transverse 0.00100 - 0.00500 cm/cm0.00100 - 0.00500 in/inAverage value: 0.00428 cm/cm Grade Count:14
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 58.0 - 93.058.0 - 93.0Average value: 76.8 Grade Count:4
Tensile Strength, Ultimate 88.0 - 180 MPa12800 - 26100 psiAverage value: 127 MPa Grade Count:16
 20.0 - 190 MPa
@Temperature -40.0 - 250 °C
2900 - 27600 psi
@Temperature -40.0 - 482 °F
Average value: 85.1 MPa Grade Count:3
 20.0 - 190 MPa
@Thickness 1.00 - 4.00 mm
2900 - 27600 psi
@Thickness 0.0394 - 0.157 in
Average value: 85.1 MPa Grade Count:3
Elongation at Break 0.600 - 3.30 %0.600 - 3.30 %Average value: 1.37 % Grade Count:16
 0.300 - 0.900 %
@Temperature -40.0 - 250 °C
0.300 - 0.900 %
@Temperature -40.0 - 482 °F
Average value: 0.633 % Grade Count:2
 0.300 - 0.900 %
@Thickness 1.00 - 4.00 mm
0.300 - 0.900 %
@Thickness 0.0394 - 0.157 in
Average value: 0.633 % Grade Count:2
Modulus of Elasticity 12.0 - 24.5 GPa1740 - 3550 ksiAverage value: 18.7 GPa Grade Count:14
 6.00 - 27.0 GPa
@Temperature -40.0 - 250 °C
870 - 3920 ksi
@Temperature -40.0 - 482 °F
Average value: 15.6 GPa Grade Count:3
 6.00 - 27.0 GPa
@Thickness 1.00 - 4.00 mm
870 - 3920 ksi
@Thickness 0.0394 - 0.157 in
Average value: 15.6 GPa Grade Count:3
Flexural Yield Strength 158 - 260 MPa22900 - 37700 psiAverage value: 196 MPa Grade Count:16
 10.0 - 300 MPa
@Temperature -40.0 - 250 °C
1450 - 43500 psi
@Temperature -40.0 - 482 °F
Average value: 121 MPa Grade Count:3
 10.0 - 300 MPa
@Thickness 0.790 - 4.00 mm
1450 - 43500 psi
@Thickness 0.0311 - 0.157 in
Average value: 121 MPa Grade Count:3
Flexural Modulus 10.0 - 24.0 GPa1450 - 3480 ksiAverage value: 17.3 GPa Grade Count:16
 5.00 - 25.5 GPa
@Temperature -40.0 - 250 °C
725 - 3700 ksi
@Temperature -40.0 - 482 °F
Average value: 13.8 GPa Grade Count:3
 5.00 - 25.5 GPa
@Thickness 0.790 - 4.00 mm
725 - 3700 ksi
@Thickness 0.0311 - 0.157 in
Average value: 13.8 GPa Grade Count:3
Compressive Yield Strength 21.3 - 152 MPa3090 - 22000 psiAverage value: 88.4 MPa Grade Count:5
Compressive Modulus 18.0 - 21.0 GPa2610 - 3050 ksiAverage value: 19.8 GPa Grade Count:3
Izod Impact, Notched 0.588 - 2.50 J/cm1.10 - 4.68 ft-lb/inAverage value: 1.38 J/cm Grade Count:5
Izod Impact, Unnotched 3.16 - 6.53 J/cm5.92 - 12.2 ft-lb/inAverage value: 4.80 J/cm Grade Count:4
Izod Impact, Notched (ISO) 8.00 - 16.0 kJ/m²3.81 - 7.61 ft-lb/in²Average value: 10.9 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.00 - 1.90 J/cm²4.76 - 9.04 ft-lb/in²Average value: 1.64 J/cm² Grade Count:8
 1.20 - 1.30 J/cm²
@Temperature -30.0 - -30.0 °C
5.71 - 6.19 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.27 J/cm² Grade Count:4
Charpy Impact, Notched 0.360 - 1.20 J/cm²1.71 - 5.71 ft-lb/in²Average value: 0.905 J/cm² Grade Count:12
 0.800 - 1.00 J/cm²
@Temperature -30.0 - -30.0 °C
3.81 - 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.950 J/cm² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cm1.00e+12 - 1.00e+16 ohm-cmAverage value: 3.00e+15 ohm-cm Grade Count:12
Surface Resistance 1.00e+11 - 1.00e+17 ohm1.00e+11 - 1.00e+17 ohmAverage value: 9.84e+15 ohm Grade Count:11
Dielectric Constant 3.40 - 5.003.40 - 5.00Average value: 4.32 Grade Count:13
 5.20 - 5.60
@Temperature 120 - 200 °C
5.20 - 5.60
@Temperature 248 - 392 °F
Average value: 5.37 Grade Count:2
 5.20 - 5.60
@Frequency 60.0 - 1.00e+6 Hz
5.20 - 5.60
@Frequency 60.0 - 1.00e+6 Hz
Average value: 5.37 Grade Count:2
Dielectric Strength 21.0 - 45.0 kV/mm533 - 1140 kV/inAverage value: 31.0 kV/mm Grade Count:11
 20.0 - 40.0 kV/mm
@Temperature 100 - 200 °C
508 - 1020 kV/in
@Temperature 212 - 392 °F
Average value: 27.6 kV/mm Grade Count:3
 20.0 - 40.0 kV/mm
@Thickness 0.800 - 3.20 mm
508 - 1020 kV/in
@Thickness 0.0315 - 0.126 in
Average value: 27.6 kV/mm Grade Count:3
Dissipation Factor 0.00600 - 0.03100.00600 - 0.0310Average value: 0.0172 Grade Count:13
 0.00800 - 0.0830
@Temperature 120 - 200 °C
0.00800 - 0.0830
@Temperature 248 - 392 °F
Average value: 0.0226 Grade Count:2
 0.00800 - 0.0830
@Frequency 60.0 - 1.00e+6 Hz
0.00800 - 0.0830
@Frequency 60.0 - 1.00e+6 Hz
Average value: 0.0226 Grade Count:2
Arc Resistance 180 - 182 sec180 - 182 secAverage value: 181 sec Grade Count:3
Comparative Tracking Index 150 - 250 V150 - 250 VAverage value: 192 V Grade Count:11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.00 - 15.0 µm/m-°C1.11 - 8.33 µin/in-°FAverage value: 4.91 µm/m-°C Grade Count:12
 -1.00 - 7.00 µm/m-°C
@Temperature 55.0 - 260 °C
-0.556 - 3.89 µin/in-°F
@Temperature 131 - 500 °F
Average value: 2.88 µm/m-°C Grade Count:4
 -1.00 - 7.00 µm/m-°C
@Thickness 2.00 - 4.00 mm
-0.556 - 3.89 µin/in-°F
@Thickness 0.0787 - 0.157 in
Average value: 2.88 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 17.0 - 80.0 µm/m-°C9.44 - 44.4 µin/in-°FAverage value: 55.1 µm/m-°C Grade Count:12
 76.0 - 100 µm/m-°C
@Temperature 55.0 - 260 °C
42.2 - 55.6 µin/in-°F
@Temperature 131 - 500 °F
Average value: 83.8 µm/m-°C Grade Count:4
 76.0 - 100 µm/m-°C
@Thickness 2.00 - 4.00 mm
42.2 - 55.6 µin/in-°F
@Thickness 0.0787 - 0.157 in
Average value: 83.8 µm/m-°C Grade Count:4
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°FAverage value: 1.50 J/g-°C Grade Count:3
Thermal Conductivity 0.320 - 0.400 W/m-K2.22 - 2.78 BTU-in/hr-ft²-°FAverage value: 0.357 W/m-K Grade Count:3
Melting Point 280 - 357 °C536 - 675 °FAverage value: 338 °C Grade Count:14
Deflection Temperature at 1.8 MPa (264 psi) 240 - 315 °C464 - 599 °FAverage value: 285 °C Grade Count:16
Deflection Temperature at 8.0 MPa 203 - 271 °C397 - 520 °FAverage value: 233 °C Grade Count:3
UL RTI, Electrical 130 - 240 °C266 - 464 °FAverage value: 210 °C Grade Count:5
UL RTI, Mechanical with Impact 130 - 210 °C266 - 410 °FAverage value: 189 °C Grade Count:5
UL RTI, Mechanical without Impact 130 - 240 °C266 - 464 °FAverage value: 209 °C Grade Count:4
Flammability, UL94 V-0V-0Grade Count:14
Oxygen Index 33.0 - 45.0 %33.0 - 45.0 %Average value: 40.2 % Grade Count:5
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 370 °C68.0 - 698 °FAverage value: 143 °C Grade Count:7
Die Temperature 290 - 370 °C554 - 698 °FAverage value: 344 °C Grade Count:7
Melt Temperature 270 - 375 °C518 - 707 °FAverage value: 342 °C Grade Count:14
Mold Temperature 30.0 - 160 °C86.0 - 320 °FAverage value: 87.0 °C Grade Count:9
Drying Temperature 150 - 170 °C302 - 338 °FAverage value: 151 °C Grade Count:13
Moisture Content 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:12
Injection Pressure 50.0 - 150 MPa7250 - 21800 psiAverage value: 100 MPa Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled

O2245 / 77948

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.